Heramid? A GRI 7645 ECP1904
Polyamide 66
PA66 15% mineral filled injection moulding grade. Heat stabilized. Toughened. Grey colour.
Post-industrial grade produced with selected polymers coming from polymerization, fibres and compounding plants.
ISO 1043 : PA66-I MX15
| Filler / Reinforcement | |
| Additive | |
| Recycled Content | |
| Features | |
| RoHS Compliance | |
| Appearance | |
| Processing Method | |
| Resin ID (ISO 1043) | |
| Tensile Modulus | 508000 | psi | ISO 527-2/1A/1 |
| Tensile Stress (Break) | 10200 | psi | ISO 527-2/1A/5 |
| Nominal Tensile Strain at Break | 10 | % | ISO 527-2/1A/50 |
| Flexural Modulus 2 | 464000 | psi | ISO 178 |
| Flexural Stress 2 | 16000 | psi | ISO 178 |
| Charpy Notched Impact Strength (73°F) | 3.8 | ft·lb/in2 | ISO 179/1eA |
| Charpy Unnotched Impact Strength (73°F) | 38 | ft·lb/in2 | ISO 179/1eU |
| Heat Deflection Temperature (264 psi, Unannealed) | 176 | °F | ISO 75-2/Af |
| Vicat Softening Temperature | 194 | °F | ISO 306/B50 |
| Melting Temperature 3 | 509 | °F | ISO 11357 |
| Drying Temperature - Desiccant Dryer | 176 | °F |
|
| Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr |
|
| Dew Point - Desiccant Dryer | < -4 | °F |
|
| Suggested Max Moisture | 0.15 | % |
|
| Processing (Melt) Temp | 536 to 572 | °F |
|
| Mold Temperature | 176 to 212 | °F |
|
| Injection Rate | Moderate-Fast |
|
|