Manufacturer: SOLVAY
Produced At: Import/ China
Product Category: Amodel PPA
Product No: Amodel HFFR-4133
Product Quantity: 25KG / BAG
Product Features: Creep Resistant.Electrically Insulating,Fatigue Resistant,High Impact Resistance,High Temperature Stiffness,Low CLTE,Low Shrinkage,Low Warpage
Amodel? LF-1950 HS
Black: Amodel? LF-1950 HS BK545
Natural: Amodel? LF-1950 HS NT
Filler / Reinforcement |
|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
Density | 1.61 | -- | g/cm3 | ISO 1183 |
Molding Shrinkage | 0.25 | -- | % | Internal Method |
Water Absorption (Equilibrium, 73°F, 50% RH) | 0.80 | -- | % | ISO 62 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
Tensile Modulus | ISO 527-2 | |||
73°F | 2.68E+6 | 2.65E+6 | psi | |
194°F | 2.39E+6 | -- | psi | |
248°F | 1.52E+6 | -- | psi | |
Tensile Stress | ISO 527-2 | |||
Break, 73°F | 39900 | 37700 | psi | |
Break, 194°F | 30500 | -- | psi | |
Break, 248°F | 19600 | -- | psi | |
Tensile Strain (Break) | 2.0 | 2.0 | % | ISO 527-2 |
Flexural Modulus (73°F) | 2.54E+6 | -- | psi | ISO 178 |
Flexural Stress | 59500 | -- | psi | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
Charpy Notched Impact Strength(73°F) | 17 | -- | ft·lb/in2 | ISO 179 |
Charpy Unnotched Impact Strength(73°F) | 38 | -- | ft·lb/in2 | ISO 179 |
| Thermal | Dry | Conditioned | Unit | Test Method |
Heat Deflection Temperature | ||||
66 psi, Unannealed | 572 | -- | °F | ISO 75-2/B |
264 psi, Unannealed | 545 | -- | °F | ISO 75-2/A |
Thermal Conductivity | 2.4 | -- | Btu·in/hr/ft2/°F | ISO 22007 |
Coefficient of Linear Thermal Expansion | 1.1 | -- | in^-5/in/°F | ISO 7991 |
| Electrical | Dry | Conditioned | Unit | Test Method |
Surface Resistivity | 1.0E+13 | -- | ohms | ASTM D257 |
Dielectric Strength | 890 | -- | V/mil | IEC 60243-1 |
Comparative Tracking Index | 600 | -- | V | IEC 60112 |
| Injection | Dry | Unit | |
Drying Temperature | 248 | °F | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.030 to 0.060 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 608 to 644 | °F | |
Middle Temperature | 617 to 644 | °F | |
Front Temperature | 617 to 644 | °F | |
Nozzle Temperature | 617 to 653 | °F | |
Processing (Melt) Temp | < 653 | °F | |
Mold Temperature | 266 to 320 | °F | |
| Injection Notes | |||
Pre-Drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 20% and only regrind of optimum quality should be used. In any case, part properties should be checked. | |||
Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields